EN 10025 S235JRak asye kabòn S275JR yo souvan itilize materyèl asye. Soti nan klas asye yo tèt yo, nou ka reyalize tou fòs nan asye kabòn S275JR pi wo pase sa yo ki an asye EN 10025 S235JR. Anba a se pou EN 10025 S235JR VS S275JR kabòn asye.

EN 10025 S235JR VS S275JR kabòn asye nan konpozisyon chimik:
| Klas | C (t mwens pase oswa egal a 16mm) | Mn | P | S | Cu | N |
| S235JR | 0.19 maksimòm | 1.50 max | 0.045 max | 0.045 max | 0.60 max | 0.014 max |
| S275JR | 0.24 max | 1.60 max | 0.045 max | 0.045 max | 0.60 max | 0.014 max |
EN 10025 S235JR VSS275JR kabòn asyenan pwopriyete mekanik:
| Klas | Fòs sede ReH/(N/mm2) (t mwens pase oswa egal a 16mm) min | Fòs rupture Rm/(N/mm2) (3mm mwens pase oswa egal a t mwens pase oswa egal a 16mm) | Elongasyon A/% (3mm mwens pase oswa egal a t mwens pase oswa egal a 40mm) min | Tès Charpy V | |
| Tanperati / degre | Enèji enpak (longitudinal)/J min | ||||
| S235JR | 235 | 360-510 | 26 | 20 | 27 |
| S275JR | 275 | 410-560 | 23 | 20 | 27 |
Kontni kabòn nan asye kabòn S275JR pi wo pase sa yo ki nan asye EN 10025 S235JR, ki asire ansyen an gen pi wo fòs. EN 10025 S235JR ak S275JR kabònplak asyeyo pwodwi pa konplètman touye pwosesis asye, ak apwovizyone nan nòmalize oswa kontwole kondisyon woule.