Anviwònman biwo gwoup GNEE
fwotman reziste plak asye pwodwi Entwodiksyon
XAR 400 fwotman asye rezistan ak XAR 500 asye reziste mete yo se plak asye ki reziste ak segondè rezistans mete.
XAR 400 fwotman asye: klas asye sa a se klas asye ki pi souvan itilize òdinè ki reziste. Li gen ekselan fòmabilite frèt ak soudabilite, ak rezistans mete li yo pa pral deteryore lè tanperati a pi ba pase 400 degre.
XAR 500 mete plak asye ki reziste: Kenbe fòmabilite ak soudabilite, ajoute eleman B, gen pi wo rezistans mete, apwopriye pou transporteurs, brwayeur, kamyon, elatriye. Trempe dlo yo ta dwe te pote soti sou livrezon.
mete plak ki reziste

fwotman asye Detay pwodwi
XAR 400 500 Plak asye Konpozisyon chimik:
Steel Klas |
C max |
sizo |
Mn |
P |
S |
Kr |
Mouvman |
B |
|---|---|---|---|---|---|---|---|---|
XAR 400 |
0.20 |
0.80 |
1.50 |
0.02 |
0.007 |
1.0 |
0.5 |
0.005 |
XAR 500 |
0.28 |
0.80 |
1.50 |
0.025 |
0.010 |
1.0 |
0.5 |
0.005 |
XAR 400 500 Pwopriyete mekanik plak asye:
Steel Klas |
Fòs Tensile Mpa |
Sede Fòs Mpa |
% elongasyon |
HB |
|---|---|---|---|---|
| XAR400 | 1300 | 1150 | Pi gran pase oswa egal a 12 | 360-440 |
| XAR500 | 1600 | 1500 | Pi gran pase oswa egal a 9 | 450-530 |
XAR 400 500 Dite plak asye ak epesè:
Steel Klas |
Kondisyon livrezon |
Epesè (mm) |
Dite (HBW) |
|---|---|---|---|
| XAR 400 | Trempe ak apeze | 3-100 | 370-430 |
| XAR 500 | 4-100 | 470-530 |
mete asye ki reziste

Gwoup GNEE resevwa kliyan k ap vizite yo
Rezo nou an kouvri tout kontinan yo, fasilite tranzaksyon transfontyè lis ak efikas. Kèlkeswa kote ou ye, GNEE asire aksè san pwoblèm ak bon jan kalite solisyon asye.
mete asye plak

Si ou gen plis bezwen ak kesyon sou asye, tanpri kontakte nou!
Baj popilè: xar 500 xar 400 abrasion reziste plak asye, Lachin xar 500 xar 400 abrasion rezistan asye plak manifaktirè, Swèd, faktori